Graphite nanorods were prepared by chemical vapor deposition of methane at temperatures from 865 degrees C to 930 degrees C using a Fe based catalyst, and were characterized by XRD, TEM and Raman spectroscopy. Results indicate that the product consists of high purity graphite nanorods with average diameters around 16...